Varnish fairing priming epoxy projects covering everything from safety equipment conditions and application techniques.
Total boat table top epoxy instructions.
Depth of color will vary depending on the amount of ink added.
Seal the wood with one or two thin coats of mixed epoxy to prevent air bubbles when you pour the epoxy in layers.
Repairing and restoring rotted wood is easy with totalboat penetrating epoxy because it glues wood fibers back together and seals wood pores to stop rot and prevent future rot.
Remove surface bubbles by waving a hair dryer or heat gun quickly back and forth just above the surface.
Tabletop epoxy quantities of 64 128 ounces typically require 5 8 minutes use a timer.
Combine 1 part totalboat tabletop epoxy and 1 part tabletop hardener by volume 100 83 by weight in a clean mixing cup.
Step 5 apply a thin seal coat.
Step 1 level your table top.
Stir thoroughly 2 3 minutes.
Add our fillers to the resin hardener mix to get a strong adhesive or a fairing and filleting compound that sands easily once cured.
First add the colors you want to the mixed epoxy then add drops of the white on top.
Add a few drops of liquid white opaque pigment until mixture is solid white.
Use a clean rag.
The key is to mix penetrating epoxy in small batches mix only as much as you can apply in 20 minutes.
For a droplet effect.
Recoat after 4 6 hours up to 12 hours directly on the previous layer.
Step 3 build the river table mold.
For a translucent effect.
See the technical data sheet for detailed instructions.
Build a mold to contain your wood and epoxy.
Do not mix any longer than 8 10 minutes.
Mix time varies by the volume of product being mixed.
Totalboat tabletop epoxy is self leveling but make sure your table is level before you.
Let cure 24 hours before use or before removing.
Get unbeatable value and great results.
We know what works and what doesn t.
Add alcohol inks to your mixed epoxy and stir until mixed thoroughly.
Step 2 clean sand the top.
It s important to remove contaminants so your epoxy will stick properly.
Pour into a second cup and stir for 2 3 minutes.
A folding motion combined with stirring and scraping the mixing vessel sides will allow you to thoroughly combine the two parts.
The white ink is heavier than the other pigments and will weigh them down and sink them.
Totalboat 5 1 epoxy cures to a high strength water resistant solid ideal for use in a variety of epoxy repair and fiberglass projects including coating bonding and laminating.